The blends of ground rubber tires (> 50 wt%) and thermoplastics have been obtained under conditions of high temperature shear deformation and characterized. The elongation at break of the blends is higher than 100%.
Реферативные базы данных:
Тип публикации:
Статья
Язык публикации: английский
Образец цитирования:
E. V. Prut, L. A. Zhorina, D. D. Novikov, A. Ya. Gorenberg, L. V. Vladimirov, A. A. Berlin, “Structure and properties of blends based on ground rubber tires and thermoplastics”, Mendeleev Commun., 27:4 (2017), 405–406